These 100-pack of 17 x 19in metal-in static shield bags feature a film printing process per MIL-PRF-81705E section 3.6 standards. This buried layer will not rub off or remove with chemicals, like IPA.
These 100-pack of 17 x 19in metal-in static shield bags feature a film printing process per MIL-PRF-81705E section 3.6 standards. This buried layer will not rub off or remove with chemicals, like IPA.
This features bags that are converted per MIL-DTL-117H if the bag size allows or is requested otherwise.
Features
Tensile Strength | Typical Value: 4,100psi, 28mPa; Testing Method: ASTM D882 |
Puncture Resistance | Typical Value: 19lbs, 85N; Testing Method: MIL-STD-3010 Method |
Seam Strength | Typical Value: 19lbs/in; Testing Method: ASTM F88 |
Thickness | Typical Value: 4.5mils, 0.114mm ±10%; Testing Method: ASTM D2103 |
WVTR | Typical Value: 0.0005g/100in2/day at 90% RH, 40°C; Testing Method: ASTM F12t49 |
OTR | Typical Value: 0.0005cc/100in2/day at 0% RH, 23°C; Testing Method: ASTM D3985 |
EMI Attenuation | Typical Value: ≥ 30dB; Testing Method: MIL-PRF-81705E |
ESD Shielding | Typical Value: 0.45V; Testing Method: EIA-541 Appendix |
Surface Resistivity - Interior | Typical Value: ≤ 1 x 10&sup5; to < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E |
Surface Resistivity - Exterior | Typical Value: < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E |
Static Decay | Typical Value: ≥ 1 second; Testing Method: MIL-PRF-81705E |
Temperature/td> | 375°F (191°C) |
Time | 1 second |
Pressure | 40psi, 276kPa |
Tensile Strength | Typical Value: 4,100psi, 28mPa; Testing Method: ASTM D882 |
Puncture Resistance | Typical Value: 19lbs, 85N; Testing Method: MIL-STD-3010 Method |
Seam Strength | Typical Value: 19lbs/in; Testing Method: ASTM F88 |
Thickness | Typical Value: 4.5mils, 0.114mm ±10%; Testing Method: ASTM D2103 |
WVTR | Typical Value: 0.0005g/100in2/day at 90% RH, 40°C; Testing Method: ASTM F12t49 |
OTR | Typical Value: 0.0005cc/100in2/day at 0% RH, 23°C; Testing Method: ASTM D3985 |
EMI Attenuation | Typical Value: ≥ 30dB; Testing Method: MIL-PRF-81705E |
ESD Shielding | Typical Value: 0.45V; Testing Method: EIA-541 Appendix |
Surface Resistivity - Interior | Typical Value: ≤ 1 x 10&sup5; to < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E |
Surface Resistivity - Exterior | Typical Value: < 1 x 10¹2;Ω/sq; Testing Method: MIL-PRF-81705E |
Static Decay | Typical Value: ≥ 1 second; Testing Method: MIL-PRF-81705E |
Temperature/td> | 375°F (191°C) |
Time | 1 second |
Pressure | 40psi, 276kPa |